Description of Product
Electro-hydraulic universal testing machine
What it does:
The electro-hydraulic servo universal testing machine WES series adopts hydraulic power as driving system, electro-hydraulic servo control, computer data acquisition and processing, which can realize closed-loop control and automatic detection. It satisfies the standard test of mechanical properties of metals, nonmetallic test regulations, the test is according to other standards of different materials or products, such as tensile, compression, bending, shear type test, can calculate the tensile strength, yield strength and extension strength, modulus of elasticity and other performance indicators of measured material. It can achieve closed-loop control such as equal rate loading, equal rate deformation, equal rate displacement, equal rate strain, etc.
Applications:
Tensile, compression, bending and shear tests of metallic and non-metallic materials
Determination of tensile strength, yield strength, elongation and elastic modulus
Closed-loop control at equal rate loading, deformation, displacement and strain
Bolt tension, bar/plate bending and bar shear tests with optional fixtures

Standards
- ISO 6892-1 - Metallic materials - Tensile testing, Part 1: Method of test at room temperature
- ISO 7500-1 - Verification of static uniaxial testing machines, Part 1: Tension/compression testing machines
Specification
WES-100B
|
Max load capacity |
100kN |
|
Load measurement range |
10-100% |
|
Accuracy class |
0.5 |
|
Resolution |
0.01kN |
|
Maximum tensile/compression space |
Tensile ≤650mm, Compression ≤550mm |
|
Thickness of flat specimen |
0-15mm |
|
Diameter of round specimen |
6-20mm |
|
Cylinder diameter |
80mm |
|
Piston stroke |
200mm |
|
Compression plate size |
Φ148mm |
|
Lifting speed of middle beam (mm/min) |
≤300mm/min |
|
Power supply |
AC380V±10V/50Hz |
|
Total power |
1.5kW(Oil pump motor 0.75kW) |
|
Host dimensions |
610×520×1650mm |
|
Control console dimensions |
1100×630×940mm |
|
Host weight |
1200kg |
WES-300B
|
Max load capacity |
300kN |
|
Load measurement range |
10-100% |
|
Accuracy class |
1 |
|
Resolution |
0.01kN |
|
Maximum tensile/compression space |
Tensile ≤650mm, Compression ≤550mm |
|
Thickness of flat specimen |
0-15mm |
|
Diameter of round specimen |
10-32mm |
|
Cylinder diameter |
125mm |
|
Piston stroke |
200mm |
|
Compression plate size |
Φ148mm |
|
Lifting speed of middle beam (mm/min) |
≤300mm/min |
|
Power supply |
AC380V±10V/50Hz |
|
Total power |
2.5kW(Oil pump motor 1.5kW) |
|
Host dimensions |
710×610×1900mm |
|
Control console dimensions |
1100×630×940mm |
|
Host weight |
1400kg |
WES-600B
|
Max load capacity |
600kN |
|
Load measurement range |
10-100% |
|
Accuracy class |
1 |
|
Resolution |
0.01kN |
|
Maximum tensile/compression space |
Tensile ≤700mm, Compression ≤600mm |
|
Thickness of flat specimen |
0-15mm |
|
Diameter of round specimen |
13-32mm |
|
Cylinder diameter |
170mm |
|
Piston stroke |
200mm |
|
Compression plate size |
Φ225mm |
|
Lifting speed of middle beam (mm/min) |
≤300mm/min |
|
Power supply |
AC380V±10V/50Hz |
|
Total power |
2.5kW(Oil pump motor 1.5kW) |
|
Host dimensions |
750×645×2020mm |
|
Control console dimensions |
1100×630×940mm |
|
Host weight |
1800kg |
WES-1000B
|
Max load capacity |
1000kN |
|
Load measurement range |
10-100% |
|
Accuracy class |
1 |
|
Resolution |
0.01kN |
|
Maximum tensile/compression space |
Tensile ≤700mm, Compression ≤600mm |
|
Thickness of flat specimen |
0-40mm |
|
Diameter of round specimen |
13-40mm |
|
Cylinder diameter |
220mm |
|
Piston stroke |
200mm |
|
Compression plate size |
Φ225mm |
|
Lifting speed of middle beam (mm/min) |
≤300mm/min |
|
Power supply |
AC380V±10V/50Hz |
|
Total power |
2.5kW(Oil pump motor 1.5kW) |
|
Host dimensions |
800×745×2150mm |
|
Control console dimensions |
1100×630×940mm |
|
Host weight |
2350kg |
WES-1500B
|
Max load capacity |
1500kN |
|
Load measurement range |
10-100% |
|
Accuracy class |
1 |
|
Resolution |
0.01kN |
|
Maximum tensile/compression space |
Tensile ≤700mm, Compression ≤600mm |
|
Thickness of flat specimen |
0-40mm |
|
Diameter of round specimen |
16-50mm |
|
Cylinder diameter |
290mm |
|
Piston stroke |
200mm |
|
Compression plate size |
Φ220mm |
|
Lifting speed of middle beam (mm/min) |
≤240mm/min |
|
Power supply |
AC380V±10V/50Hz |
|
Total power |
2.2kW |
|
Host dimensions |
1150×1000×2750mm |
|
Control console dimensions |
1100×630×940mm |
|
Host weight |
4800kg |
WES-2000B
|
Max load capacity |
2000kN |
|
Load measurement range |
10-100% |
|
Accuracy class |
1 |
|
Resolution |
0.01kN |
|
Maximum tensile/compression space |
Tensile ≤800mm, Compression ≤650mm |
|
Thickness of flat specimen |
0-50mm |
|
Diameter of round specimen |
20-70mm |
|
Cylinder diameter |
300mm |
|
Piston stroke |
250mm |
|
Compression plate size |
Φ220mm |
|
Lifting speed of middle beam (mm/min) |
≤300mm/min |
|
Power supply |
AC380V±10V/50Hz |
|
Total power |
3kW |
|
Host dimensions |
1200×1050×2923mm |
|
Control console dimensions |
1100×630×940mm |
|
Host weight |
6800kg |
FAQ
Q: What tests can the WES series electro-hydraulic servo universal testing machine perform?
A: It performs tensile, compression, bending and shear tests on metallic and non-metallic materials, and calculates tensile strength, yield strength, elongation, elastic modulus and other performance indicators. Optional fixtures allow bolt tension, bar/plate bending and bar shear tests.
Q: What load capacities are available for the WES series?
A: Six models are available: WES-100B (100kN), WES-300B (300kN), WES-600B (600kN), WES-1000B (1000kN), WES-1500B (1500kN) and WES-2000B (2000kN). Accuracy class is 0.5 for WES-100B and 1 for the other models; resolution is 0.01kN.