Rapid Chloride Permeability Test RCPT Apparatus

Rapid Chloride Permeability Test RCPT Apparatus

Model: DTL-A
Standard: ASTM C1202
AASHTO T277

 

Description
Standards
Specification
Features
Video
Documents
FAQ

 

Description of Product

Rapid chloride permeability test RCPT apparatus

What it does:

This test method allows evaluation of chloride permeability characteristics of concrete. The test is performed to monitor the amount of electrical current passing through concrete cores or cylinders. A potential difference is maintained across the ends of the specimen, one of which is the negative end and is immersed in a sodium chloride solution, the other (positive end) in a sodium hydroxide solution. The total charge passed, in Coulombs, that is related to the resistance of the specimen to chloride ion penetration is measured.

How it works:

Closed loop maintained 60 V DC potential difference, passed current measured and integrated relative to time.

Applications:

Evaluation of chloride permeability characteristics of concrete

Monitoring the amount of electrical current passing through concrete cores or cylinders

Measuring the total charge passed in Coulombs to indicate resistance to chloride ion penetration

Rapid chloride permeability test RCPT apparatus

Standards

 

  • ASTM C1202 - Electrical Indication of Concrete's Ability to Resist Chloride Ion Penetration
  • AASHTO T277 - Electrical Indication of Concrete's Ability to Resist Chloride Ion Penetration

 

Specification

 

Test ability

C30~C50 Portland cement concrete

Test channel

6 channels, 9 channels, 12 channels, 16 channels optional

Working environment

0℃~50℃ humidity≤75%

Measurement error

<1%

Accuracy

± 0.1 V, ± 1 mA

Working voltage

~220VAC 60VDC

Working current

0-360mA

Host

385×345×145mm, 5kg

Specimen cells

6 sets; 440×350×210mm; 9kg

Total weight

46kg(vacuum saturated machine included)

 

VACUUM SATURATED MACHINE

Volume

10L

Vacuum accuracy

±0.001Mpa

Power

300W

Power Supply

AC 220V

Console Voltage

DC 5V

Transmitter Voltage

DC 24V

Dimension

750×680×400 mm

Weight

32 kg

 

Features

 

● Embedded computer control, power outages and power-down data storage, advanced technology, well-made, reliable performance, high accuracy

 

● LCD display, with real-time display/print and analysis function, can be separated from Pc to use directly, to facilitate the outdoor field detection.

 

● Standard RS232 serial communications with fully automatic PC connection software can output the flux test report to generate curve, and then print for analysis and archiving

 

● Automatic short circuit protection to avoid equipment damage

 

● Imported material fixture, high accuracy, easy and smart to use

 

● Can simultaneously test two groups (6), three (9), four (12) or five (16) concrete block one time

 

● With the latest smart-in-one vacuum saturated machine

 

Video

 

 

FAQ

Q: What does the RCPT apparatus measure?

A: It evaluates chloride permeability characteristics of concrete by monitoring the electrical current passing through concrete cores or cylinders and measuring the total charge passed in Coulombs. A closed loop 60 V DC potential difference is maintained across the specimen.

Q: Which standards and test channels does it support?

A: It conforms to ASTM C1202 and AASHTO T277 and supports 6, 9, 12 or 16 channels. It tests C30~C50 Portland cement concrete with measurement error under 1%.

 