Zhuozhou Tianpeng Imp. and Exp. Trade Co., Ltd. is one of the leading manufacturers and suppliers of automatic penetrometer in China. With abundant experience, we warmly welcome you to buy customized automatic penetrometer made in China here from our factory. Quality products and reasonable price are available.
Description of Product
This automatic penetrometer features a touch screen interface, motorized fast needle adjustment for precise positioning, and an integrated constant temperature bath with ±0.1℃ accuracy. The instrument automatically calculates penetration index PI, equivalent softening point T800 and equivalent brittle point T1.2. A built-in 485 interface supports real-time data networking. Suitable for road asphalt, modified bitumen and related materials.

Specification
TECHNICAL PARAMETERS
|
Measuring range |
0~450 penetration |
|
Temperature measuring range |
0.00~50.00°C |
|
Temperature control range |
15°C lower than ambient temperature~50°C |
|
Resolution |
0.01°C |
|
Temperature control accuracy |
≤±0.1°C |
|
Time control |
0-60 seconds (arbitrary setting) |
|
Displacement control |
Adopting high-precision LVDT displacement sensor, split structure, no friction when the needle bar falls. |
|
Measuring range |
0-50mm |
|
Resolution |
0.01mm (0.1 Penetration) |
|
Relative displacement accuracy |
≤±0.1mm |
|
Data storage |
200 groups |
|
Dimensions |
390mmx 310mm x575mm (L×W×H) |
Features
● Touch screen for intuitive operation and parameter setting..
● Fast needle adjustment driven by stepping motor and lead screw slider, enabling high-precision jogging for quick lifting.
● Internal integrated constant temperature system combines semiconductor refrigeration, cooling module, heating sheet and water circulation to maintain ±0.1℃ high-precision water bath control.
● Needle bar assembly uses standard needles from designated manufacturers, regularly verified by third parties, with needle quality strictly meeting 2.5±0.05g specification requirements.
● Powerful data processing capability automatically calculates penetration index PI, equivalent softening point T800 and equivalent brittle point T1.2 from test results. Provides intelligent result analysis with user prompts. Supports online data upload and comes with 485 interface (ModBus protocol) for real-time data networking.