Zhuozhou Tianpeng Imp. and Exp. Trade Co., Ltd. is one of the leading manufacturers and suppliers of walking profilometer in China. With abundant experience, we warmly welcome you to buy customized walking profilometer made in China here from our factory. Quality products and reasonable price are available.
Description of Product
The Walking Profilometer is a high-precision measurement device designed to collect pavement surface condition data at true walking speed. It generates outputs from pavement profile, including International Roughness Index (IRI), optionally MPD texture, and distance measurements. The platform is separate from the carriage, reducing susceptibility to operator influence. Data collection can be performed at variable speeds up to 5km/hr, with operation controlled via an Android tablet. Real-time results are displayed on screen to support onsite decision-making.

TECHNICAL PARAMETERS
|
Operator quantity |
1 person |
|
Operate speed |
Normal walking speed |
|
Calculate length of the road |
Any length more than 5m |
|
Roughness index sampling interval |
12.5cm |
|
System power |
large capacity lithium battery |
|
Operate environment temperature |
- 40℃ ~ 80℃ |
|
Dimensions |
650mm×380mm×330mm |
|
Weight |
20Kg |
Measurable Parameters
|
International Roughness Index (IRI) |
|
is an indicator used worldwide for the characterization of longitudinal road roughness. This study summarized IRI limit values for new, reconstructed or rehabilitated roads, for in-service (existing)roads and road classification schemes used around the world. |
|
Flatness standard deviation (σ) |
|
standard deviation of the flatness adopt continuous flatness meter to measure the standard deviation of unflatness, represents the flatness of the road surface. |
|
Ride Number(RN) |
|
The Ride Number (RN) is a mathematical processing of longitudinal profiles that allows the estimation of the subjective ride quality perceived by road users. |
|
Ride Quality Index (RQI) |

Features
- Classified as a World Bank Class 1 profilometry device for high-accuracy pavement profiling
- Optional laser module available for MPD texture measurement to support surface characterization
- Supports variable data collection speeds for flexible testing under different site conditions
- Operated via Android tablet with intuitive interface for simplified field control
- Features Bluetooth connectivity for wireless data transfer and remote operation
- Outputs ERD and PPF file formats compatible with ProVAL software for detailed analysis

Application
1. Provides outputs of IRI, longitudinal profile and distance
2. Reference tool for calibrating and assessing high speed profilers
3. Suitable for many surfaces, including paved roads and footpaths, airfields and runways, bridges and carparks.
Documents
Hot Tags: walking profilometer, China walking profilometer manufacturers, suppliers, factory