Zhuozhou Tianpeng Imp. and Exp. Trade Co., Ltd. is one of the leading manufacturers and suppliers of concrete air meters in China. With abundant experience, we warmly welcome you to buy customized concrete air meters made in China here from our factory. Quality products and reasonable price are available.
Description of Product
A widely used kit for determining entrained air content in fresh concrete. Provides fast, accurate results whether sampling from the truck or chute. Includes all components required for testing and calibration. Operates by equalizing known air volume in the pressure chamber with unknown entrained air in the concrete sample.

Standards
- EN 12350-7
- BS 1881-106
- ASTM C231
Specification
TECHNICAL PARAMETERS
LC-615
|
Capacity (L) |
7 |
|
Air content range |
1-10% |
|
Accuracy |
± 0.1%(1%-8% of air content); 0.2%(8%-10% of air content) |
|
Dimensions(mm) |
Standard consolidation cells with upper and lower, porous discs with cutting rings (different sizes), Material: tin bronze Dia.50mm |
|
Slotted steel weight set |
Dia. 330 x 500 |
|
Weight(Kg) |
10 |
LS-546
|
Capacity (L) |
1 |
|
Air content range |
0-20% |
|
Accuracy |
± 0.1%(1%-8% of air contentof air content); ± 0.3%(12%-20% of air content) |
|
Dimensions(mm) |
Dia. 200 x 320 |
|
Weight(Kg) |
4 |
LA-0316
|
Capacity (L) |
7 |
|
Air content range |
0-10% |
|
Accuracy |
± 0.1%(1%-6% of air content); 0.2%(6%-10% of air content) |
|
Dimensions(mm) |
Dia. 200 x 320 |
|
Weight(Kg) |
10 |
B-2030
|
Capacity (L) |
1 |
|
Air content range |
0-50% |
|
Accuracy |
± 0.1% |
|
Dimensions(mm) |
Dia. 200 x 320 |
|
Weight(Kg) |
4 |
Features
● Industry-standard kit for measuring entrained air content in fresh concrete, delivering fast and accurate results directly on site
● Complete set includes everything needed for testing and maintaining calibration
● Operates on Boyle's law principle by equalizing known air volume in pressure chamber with unknown entrained air in concrete sample
● Pressure gauge displays air content as direct percentage to nearest 0.1%
● Also known as "Type B" meter, conforming to ASTM test methods
● Consists of two main components: machined cast aluminum base (measuring chamber) and cover assembly with pressure gauge, air pump and valves
● Base can also be used for unit weight measurement of fresh concrete and aggregates
● Designed for easy disassembly and field maintenance with replaceable O-rings and parts
● Machine-finished interior surfaces and rims facilitate frequent water cleaning
● Super Pump features dual O-ring seals to prevent air leakage; proper maintenance ensures reliable operation
● Supplied complete with calibration set for ongoing accuracy verification