News

How Can Cement Testing Equipment Be Used To Maximize Its Service Life?

Feb 11, 2026 Leave a message

Preventative Maintenance Plan: Daily checks of bearing temperature and vibration data.

Quarterly lubrication oil changes and weld inspections.

Spare Parts Upgrade: Replacing traditional steel with silicon carbide ceramic liners reduces vertical mill wear by 60% (according to experimental data from *Cement International*, 2023).

Capacity Matching: Avoiding prolonged operation above design capacity; for example, controlling the actual output of a 5000t/d production line to within 5500t/d.