The equipment configuration and uses of a cement testing laboratory mainly include the following:

1. Universal testing machine for testing compressive and flexural strength;

2. Cement mortar mixer for preparing standard mortar specimens;

3. Standard curing chamber for providing a constant temperature and humidity curing environment;

4. Cement paste mixer for preparing cement paste;

5. Specific surface area analyzer for measuring cement fineness;

6. Consistency meter for measuring cement paste consistency;

7. Setting time meter for testing cement setting characteristics;

8. Flowability meter for evaluating cement paste flow properties;

9. Chloride ion content analyzer for analyzing cement chemical composition.